Abstract

Thyrotherm 2999 exhibits high-temperature strength with wear resistance. This datasheet provides information on composition, physical properties, and hardness. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TS-665. Producer or source: Schmolz + Bickenbach USA Inc.