Abstract

UGINOX MA4 (X46Cr13, No. 1.4034) is an age-hardenable martensitic stainless steel, mostly used where a sharp edge for cutting is needed. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-1023. Producer or source: Arcelor Stainless Processing LLC.