Abstract

Maxival 188HS is an enhanced machining version of AISI Type 303 stainless steel. The alloy has a specified inclusion picture to enhance machining by modifying both sulfide and oxide inclusions. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and machining. Filing Code: SS-1020. Producer or source: Valbruna Stainless Inc.