Abstract

Haynes Ti-3Al-2.5V alloy is used where the strength/weight ratio is of prime importance; the alloy is 43% lighter than 21-6-9 stainless steel. It is most often used in the form of seamless tubing for aircraft hydraulic systems. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: TI-145. Producer or source: Haynes International Inc.