Supermet 2506 Cu is a rutile-coated electrode for welding copper bearing superduplex austenitic/ferritic stainless steels. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming and joining. Filing Code: SS-995. Producer or source: Metrode Products Ltd.