Abstract

Sandvik 2RK66 is recommended for springs that will operate in extremely corrosive conditions. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on low and high temperature performance as well as forming and heat treating. Filing Code: SS-992. Producer or source: Sandvik Steel Company.