Abstract
15-15HS MAX stainless is an austenitic alloy strengthened by both nitrogen and high manganese. It has a low permeability and can be considered for nonmagnetic drill collars. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-988. Producer or source: Carpenter Specialty Alloys.