Abstract

Alcan 6156 T4, T6 clad sheets were developed with weldability and high damage tolerance compared with incumbent 2024 alloy. Aerospace applications include fuselages clad sheets. This datasheet provides information on composition, physical properties, and tensile properties as well as fatigue. It also includes information on forming, heat treating, and joining. Filing Code: AL-408. Producer or source: Alcan Inc.