TLS L6 is a versatile oil-hardening tool steel with better toughness than the other alloys in its class. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as forming and heat treating. Filing Code: TS-657. Producer or source: Timken Latrobe Steel.