Abstract

The high strength of Tenform XF450, a hot-rolled high-strength low-alloy steel, allows the user to increase the strength of a finished component or to reduce the thickness. The steel is used in the construction and the automotive industries. This datasheet provides information on composition, physical properties, tensile properties. and bend strength. It also includes information on forming. Filing Code: CS-148. Producer or source: Hille & Mueller, USA Inc. See also Alloy Digest CS-173, November 2012.