Crusteel EN.30.B has a combination of toughness, through hardening, and wear resistance for applications in plastic molds. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, and joining. Filing Code: TS-634. Producer or source: Crucible Service Centers.