Abstract
Tatmo is a general-purpose high-speed steel often used in twist drills and taps. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness. It also includes information on wear resistance as well as forming, heat treating, and machining. Filing Code: TS-633. Producer or source: Timken Latrobe Steel.