Abstract
35N LT is a cobalt-base superalloy produced by a melt practice that results in improved fatigue life for wires used in the medical field. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fatigue. It also includes information on forming and heat treating. Filing Code: CO-112. Producer or source: Fort Wayne Metals.