Abstract

Metglas 2605 SA1 is an amorphous iron-base soft magnetic alloy designed for extremely low core loss at distribution and power transformer frequencies and inductions. Applications include high-frequency inductors and current transformers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, forming, and heat treating. Filing Code: FE-139. Producer or source: Metglas Inc.