Abstract

Olin Alloy C72200 is a chromium-containing copper-nickel alloy used extensively in seawater. The alloy is used for its corrosion-erosion resistance and is often called Cupronickel with Cr. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CU-745. Producer or source: Olin Brass.