Abstract

The Hiduron series of alloys are medium-strength copper-nickel alloys that offer excellent corrosion resistance and good impingement erosion resistance. Hiduron 107 is a medium-strength corrosion-resistant copper-nickel alloy that is often used in seawater applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and shear strength. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: CU-744. Producer or source: Langley Alloys.