HPM 233 is a wrought nickel with low carbon. The alloy is used in electrical and electronic components. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-635. Producer or source: Hamilton Precision Metals.