Nicrimphy 600 is a nickel-base alloy designed to offer good corrosion and oxidation resistance. It also has good mechanical properties over a wide range of temperatures. This datasheet provides information on composition, physical properties, hardness, tensile properties, and shear strength. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-633. Producer or source: Metalimphy Precision Alloys Inc.