Abstract

Carpenter 825 Plus is a corrosion-resistant alloy often used in downhole or surface gas well components. The alloy is age hardenable. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Ni-632. Producer or source: Carpenter Technology Corporation.