Abstract

Sandvik 12C27 is a martensitic stainless steel for knife applications. It is supplied in both the annealed or cold-rolled condition. This datasheet provides information on composition, microstructure, hardness, and tensile properties. It also includes information on forming and heat treating. Filing Code: SS-954. Producer or source: Sandvik Steel Company.

This content is only available as a PDF.