Phynox is a high yield strength cobalt alloy with a range of physical, chemical, and technological properties that make it useful for a wide variety of applications. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: CO-115. Producer or source: Metalimphy Precision Alloys Inc.