Abstract

Kubota alloy HH II is a heat-resistant fully austenitic stainless steel casting for multiple furnace parts. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as casting and joining. Filing Code: SS-980. Producer or source: Kubota Metal Corporation, Fahramet Division.