Boehler L330 VMR is a Ni-Mo-Cr-W alloy with outstanding corrosion resistance that is maintained even in the welded condition. It also has excellent resistance to oxidizing media. It is widely used in the severest environments encountered in chemical processing, pollution control, industrial and municipal waste treatment, and pulp and paper production. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Ni-642. Producer or source: Böhler-Uddeholm Specialty Metals Inc.
BOEHLER L330 VMR, chemical composition, chemical processing applications, corrosion-resistant alloys, elasticity, fracture toughness, heat treatability, high-temperature alloys, machinability, paper production, physical properties, pollution control applications, tensile properties, waste treatment applications, workability, thermal properties, UNS N10276
This content is only available as a PDF.
Copyright © ASM International® 2006
2006
ASM International
Topics
Pollution control devices
Waste handling and recycling
Corrosion-resistant alloys
High-temperature alloys
Nickel-molybdenum alloys
Chemical composition
Heat treatability
Machinability
Workability
Elastic modulus
Fracture toughness
Tensile properties
Physical properties
Thermal properties
Chemical and petrochemical processing equipment
Pulp and paper processing equipment
You do not currently have access to this content.