Tribaloy T-400C is a cobalt hardfacing alloy with Laves phase particles to promote wear resistance while improving corrosion and oxidation resistance over T400. This datasheet provides information on composition, hardness, tensile properties, and shear strength as well as fracture toughness. It also includes information on corrosion and wear resistance as well as casting, joining, and powder metal forms. Filing Code: CO-114. Producer or source: Deloro Stellite Company Inc.