Abstract

Ti-3Al-8V-6Cr-4Zr-4Mo alloy is a heat treatable beta grade titanium alloy. It is a high-strength alloy with fair weldability and is easier to melt than 13-11-3. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TI-94. Producer or source: Titanium alloys mills. Originally published as Ti-3Al-8V-6Cr-4Zr-4Mo BETA ALLOY, January 1990, revised June 2005.