Sandvik SANMAC 4435 is a molybdenum-containing austenitic stainless steel grade in hollow bar with a minimum molybdenum level of 2.5%. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-933. Producer or source: Sandvik Steel Company.