Crofer 22 APU is an alloy especially developed for solid oxide fuel cell applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and joining. Filing Code: SS-926. Producer or source: Thyssen VDM USA Inc.