Alloys 6605 and 6105 belong to the 6xxx series of aluminum alloys. They are medium strength alloys and are used as structural members such as handrails and ladders. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on joining and surface treatment. Filing Code: AL-393. Producer or source: Alcoa Engineered Products.