Inconel alloy 050 is an improved corrosion-resistant alloy in tubular form for down hole service. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming. Filing Code: Ni-629. Producer or source: Special Metals Corporation.