Nirosta 4561 is a very-low-carbon, stabilized with titanium, version of the molybdenum-containing corrosion-resistant austenitic stainless steels. The alloy resists exhaust gases and is used in flues. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SS-943. Producer or source: ThyssenKrupp Nirosta GmbH.