Durehete 950 is a high-strength steel bolting material often used in steam turbine and other power plant applications. It is usually supplied in the heat treated condition. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness, creep, and deformation. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: SA-145. Producer or source: Corus Products USA. Originally published May 1963, revised October 2005.