Abstract

Allvac 38-644 is a metastable beta titanium alloy known for its ductility in the solution treated condition and its high strength and ductility in the solution treated and aged condition. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TI-134. Producer or source: Allvac Metals Company.