Docol 160M is a high-strength cold-forming steel that is used for many transportation and structural products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on joining. Filing Code: SA-537. Producer or source: SSAB Swedish Steel Inc.