Abstract

Wieland-M37 has excellent cold-working properties and corrosion resistance. The alloy is used in the deep-drawn and stamped condition for electrical products. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-716. Producer or source: Wieland Metals Inc., Wieland-Werke AG.