Abstract

DUAL-TEN 600 is a dual-phase steel for the automotive industry. Dual-phase steels are most commonly used in structural applications where they have replaced more conventional high-strength low-alloy (HSLA) steels. Applications include front and rear rails, crush cans, rocker reinforcements, pillar reinforcements, inner and outer cowl, back panels, cross members, bumpers, and door intrusion beams. This datasheet provides information on composition, physical properties, microstructure, tensile properties, and bend strength as well as deformation. It also includes information on forming and joining. Filing Code: SA-533. Producer or source: United States Steel.