Wieland-M30 has excellent cold working properties and good strength. The alloy is used in decorative products. It is commonly called cartridge brass, spinning brass, or extra-quality brass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as deformation. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: CU-713. Producer or source: Wieland Metals Inc., Wieland-Werke AG.