Abstract
Docol 205DP is an ultrahigh strength steel that is used for many transportation and construction products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-540. Producer or source: SSAB Swedish Steel Inc.