Olin alloy C19020 is a phosphor bronze alloy with solid solution strengthening and very high conductivity for applications in the automotive connector market. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. Filing Code: CU-727. Producer or source: Olin Brass.