Micro-Melt PD#1 alloy is a powder metallurgically processed air hardening die steel with wear resistance better than AISI D2 while maintaining good toughness. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as forming and heat treating. Filing Code: TS-602. Producer or source: Carpenter Specialty Alloys.