Abstract

Docol 85DL is a high-strength cold-forming steel (0.10C-0.40Si) that is used for transportation and structural products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on forming and joining. Filing Code: SA-521. Producer or source: SSAB Swedish Steel Inc.