Abstract

Outokumpu 7026 (C 7026) is a high-strength age-hardenable CuNiSi alloy for demanding signal and power applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength as well as deformation. It also includes information on forming. Filing Code: CU-710. Producer or source: Outokumpu American Brass Inc.