Miller alloy MHP 101 has excellent cold working properties. The alloy is used for its combination of strength, relaxation resistance, electrical conductivity, and good formability. It is used as connectors and springs. This datasheet provides information on composition, physical properties, elasticity, and tensile properties. It also includes information on forming, heat treating, and joining. Filing Code: CU-706. Producer or source: The Miller Company.