Abstract

Outokumpu 5119, or KLF-7, is a high performance copper tin alloy with excellent combination of strength and stress relaxation resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and bend strength. Filing Code: CU-699. Producer or source: Outokumpu Copper Americas Inc.