Abstract

DuraFoil-Clad is a laminate composite form of DuraFoil (see Alloy Digest SS-892, November 2003), a heat-resistant ferritic stainless steel with excellent oxidation resistance for high-temperature applications. The material is a metallurgically bonded Al/Fe-Cr stainless steel/Al metallic composite. The material should be converted to a uniform solid-solution alloy (the single alloy form DuraFoil) by diffusion alloying before service in high-temperature applications. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as deformation. It also includes information on corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-897. Producer or source: Engineered Materials Solutions Inc.