Lukens 130 is a quenched-and-tempered general structural plate steel with a minimum yield strength of 896 MPa (130 ksi). This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming and joining. Filing Code: SA-526. Producer or source: International Steel Group Inc.