Docol 115DL is a high-strength cold-forming steel used for transportation and structural products. This datasheet provides information on composition, physical properties, tensile properties, and bend strength. It also includes information on joining. Filing Code: SA-525. Producer or source: SSAB Swedish Steel Inc.