Abstract
Algoma AR225 is a carbon steel developed primarily to supply a low-cost material for high-abrasion applications. It is furnished in the form of as-rolled plate with a relatively high carbon content (0.35-0.45%). AR-225 is sold on the basis of chemical analysis only; the number 225 signifies the approximate Brinell hardness. On thicknesses one-half inch and over, this Brinell value may be lower than 225 because of higher finishing temperatures. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on forming, heat treating, machining, and joining. Filing Code: CS-138. Producer or source: Algoma Steel Corporation Ltd.