DuraFoil is a heat-resistant ferritic stainless steel, belonging to the FeCrAl alloy or FeCr alloy family. It has excellent oxidation resistance for high temperature applications. This datasheet provides information on composition, physical properties, microstructure, hardness, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, and joining. Filing Code: SS-892. Producer or source: Engineered Materials Solutions Inc.