Datalloy 2 is an enhanced corrosion-resistant nonmagnetic stainless steel. The composition contains a high level of manganese and nitrogen to stabilize the austenite. Applications include replacement of standard chromium-manganese steels in drill string components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as machining. Filing Code: SS-862. Producer or source: Allvac Ltd.