Abstract

AlcoTec weld filler wire 4047 is a general-purpose high silicon containing wire for both welding and brazing. This datasheet provides information on composition, physical properties, and tensile properties. It also includes information on joining. Filing Code: AL-381. Producer or source: AlcoTec Wire Corporation.